Description
Hempadur Avantguard 550 is an activated zinc epoxy primer in compliance with the requirements of Level 3, type II in SSPC Paint-20, 2019. Hempadur Avantguard 550 functions as a zinc-rich epoxy featuring a higher mechanical strength. The product is in full compliance with ASTM D520 type II and EU Directive 2004/42/EC, the Paints Directive on the limitation of volatile organic compounds: subcategory j.
Recommended use
Hempadur Avantguard 550 is recommended as a versatile primer for long-term protection of steel in severely corrosive environments.
Service temperature:
Flash point: 29°C [84°F]
VOC content mixed product
Legislation | Value |
---|---|
EU | 325 g/L [2.71 lb/US gal] |
US (coatings) | 325 g/L [2.71 lb/US gal] |
US (regulatory) | 325 g/L [2.71 lb/US gal] |
China | 325 g/L [2.71 lb/US gal] |
According to specific legislation, see details in the Explanatory Notes available at Hempel website, hempel.com or at your local Hempel website.
Handling
Handle with care. Before and during use, observe safety labels on packaging and paint containers and follow all local and national safety regulations. Always consult Hempel’s Safety Data Sheet for this product along with the Product Data Sheet.
For professional use only.
Cleanliness
New build:
Roughness
Consult Hempel’s separate Surface Preparation Guidelines for more details.
Mixing ratio
Base 1734U : Curing Agent 97043 (4 : 1 by volume)
Products containing floating or settling particles/pigments need to be continuously stirred during application. This is especially important in case of heavy thinning.
Thinner
Cleaner
Pot life
Product temperature | Pot life |
---|---|
0°C [32°F] | 6 hours |
20°C [68°F] | 3 hours |
40°C [104°F] | 1 hour |
Tool | Thinning max vol. | Application parameters |
---|---|---|
Airless spray | 10% | Nozzle pressure: 220 bar [3200 psi] |
Nozzle orifice: 0.017-0.021″ |
If brush or roller application is used, more coats will be necessary to achieve the specified dry film thickness. Spray data are indicative and subject to adjustment. Pressure is for a material temperature of 20°C [68°F].
Specification range | Dry film thickness | Wet film thickness | Theoretical spreading rate |
---|---|---|---|
Low | 40 micron [1.6 mils] | 62 micron [2.5 mils] | 16 m²/L [652 sq ft/US gal] |
High | 100 micron [4.0 mils] | 154 micron [6.2 mils] | 6.5 m²/L [265 sq ft/US gal] |
Recommended | 60 micron [2.4 mils] | 92 micron [3.7 mils] | 11 m²/L [448 sq ft/US gal] |
Overthickness must be closely controlled and never locally exceed 200 micron [8.0 mils] DFT. On irregular surfaces it is recommended to employ special care in avoiding over application.
Relative Humidity:
Product compatibility
Surface temperature | Touch dry (min) | Hard dry (hours) |
---|---|---|
-10°C [14°F] | 70 | 6 |
0°C [32°F] | 40 | 4 |
20°C [68°F] | 15 | 1½ |
40°C [104°F] | 5 | ½ |
Determined for dry film thickness 60 micron [2.4 mils] at standard conditions, see Hempel’s Explanatory Notes for details.
Quality name | -10°C [14°F] | 0°C [32°F] | 20°C [68°F] | 40°C [104°F] |
---|---|---|---|---|
Atmospheric medium | ||||
Hempaprime Multi 500 Winter | Min – Max – | – | – | – |
Hempathane HS 55610 | Min – Max – | – | – | – |
Atmospheric severe | ||||
Hempaprime Multi 500 Winter | Min – Max – | – | – | – |
Hempathane HS 55610 | Min – Max – | – | – | – |
Overcoating times are indicative for products of the same generic chemistry.
Consult Hempel’s specification for more information.
Ambient temperature | Base shelf life | Curing Agent shelf life |
---|---|---|
25°C [77°F] | 12 months | 36 months |
Shelf life from date of production, when stored in original, unopened containers. Thereafter, the product quality must be re-inspected. Storage at elevated temperatures may reduce shelf life. For advice, please consult Hempel.
Dry film thickness | GWP (Global Warming Potential) |
---|---|
1 µm | 14.7 g CO₂e/m² |
1 mil | 0.077 lb CO₂e/ft² |
Includes raw materials, in-bound transport, production, and emitted VOCs.
Calculated based on the standard shade defined in this PDS. Values may vary.
Product Data Sheet – Hempadur Avantguard 550
Issued by Hempel A/S – May 2025
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations