Hempaprime Multi 500 Summer is a fast drying, high solids epoxy paint. It provides hard wearing and long lasting barrier protection in coating systems for severe corrosive environments.
Hempaprime Multi 500 Summer is recommended as a high-build, intermediate coat in high performance coating systems where fast handling and short overcoating times are required. Due to its fast drying – up to twice as fast as comparable products – the product is excellent for projects where fast throughput is key. The product can also be used as a self-priming, surface tolerant coat and a finishing coat in heavy-duty coating systems.
25°C [76°F]
Legislation | Value |
---|---|
EU | 200 g/L [1.67 lb/US gal] |
US (coatings) | 200 g/L [1.67 lb/US gal] |
US (regulatory) | 200 g/L [1.67 lb/US gal] |
China | 200 g/L [1.67 lb/US gal] |
According to specific legislation, see details in the Explanatory Notes available at Hempel website. VOC values may vary with shade, please consult the Safety Data Sheet, section 9.
Handle with care. Before and during use, observe safety labels on packaging and paint containers and follow all local and national safety regulations. Always consult Hempel’s Safety Data Sheet for this product along with the Product Data Sheet.
For professional use only.
Base 45959 : Curing Agent 95092 (4 : 1 by volume)
Stir well before use.
Hempel’s Thinner 08960 / 08450
Hempel’s Thinner 08450 / Hempel’s Tool Cleaner 99610
Product temperature | Pot life |
---|---|
20°C [68°F] | 2 hours |
30°C [86°F] | 1½ hours |
40°C [104°F] | 1 hour |
Tool | Thinning max vol. | Application parameters |
---|---|---|
Airless spray | 5% | Nozzle pressure: 225 bar [3300 psi], Orifice: 0.019-0.023″ |
Brush/Roller | 5% | Not Applicable |
If brush or roller application is used, more coats will be necessary to achieve the specified dry film thickness.
Parameter | Low | High | Recommended |
---|---|---|---|
Dry film thickness (DFT) | 100 micron [4.0 mils] | 250 micron [10 mils] | 150 micron [6.0 mils] |
Wet film thickness (WFT) | 118 micron [4.7 mils] | 295 micron [12 mils] | 177 micron [7.1 mils] |
Theoretical spreading rate | 8.5 m²/L [346 sq ft/US gal] | 3.4 m²/L [139 sq ft/US gal] | 5.7 m²/L [232 sq ft/US gal] |
– Optimal paint temperature for proper mixing, pumping and spraying is: 25°C [77°F].
– To avoid condensation, apply on a clean and dry surface with a temperature that is at least 3°C [5°F] above the dew point.
– Relative humidity must be below 85% during application.
– Relative humidity must be below 85% during curing
– Product requires heavy duty spray equipment; spray hoses shall be as short as possible.
– Metallised surfaces should be overcoated before exposure to open air conditions.
– Flash-coat technique is recommended when overcoating porous substrates.
Temp. | Touch dry | Surface dry | Hard dry | Through dry | Fully cured |
---|---|---|---|---|---|
20°C [68°F] | 90 min | 3 h | 4½ h | — | — |
30°C [86°F] | 60 min | 1¼ h | 1¾ h | 4 h | 4 d |
40°C [104°F] | 30 min | ¾ h | 1 h | — | — |
Quality name | 20°C [68°F] | 30°C [86°F] | 40°C [104°F] |
---|---|---|---|
Hempaprime Multi 500 Summer | Min 4 h / Max Ext* | 2½ h / Ext* | 2 h / Ext* |
Hempathane HS 55610 | Min 4 h / Max Ext* | 2½ h / Ext* | 2 h / Ext* |
Ext*: Extended period; consult Hempel for advice.
Overcoating times are indicative for products of the same generic chemistry.
Dry film thickness | 1 µm | 1 mil |
---|---|---|
GWP | 5.5 g CO₂e/m² | 0.029 lb CO₂e/ft² |
Covers raw materials, transport, manufacturing, VOCs emitted during/after application.
Product Data Sheet – Hempaprime Multi 500 Summer
Issued by Hempel A/S – March 2025
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations