Description
Hempadur Avantguard 770 is an activated zinc-rich epoxy primer in compliance with the requirements of Level 2, type II in SSPC Paint-20, 2019 and ISO 12944 Part 5, 2018. The product is in full compliance with ASTM D520 type II and EU Directive 2004/42/EC, the Paints Directive on the limitation of volatile organic compounds: subcategory j.
Description
Hempadur Avantguard 770 is an activated zinc-rich epoxy primer in compliance with the requirements of Level 2, type II in SSPC Paint-20, 2019 and ISO 12944 Part 5, 2018. The product is in full compliance with ASTM D520 type II and EU Directive 2004/42/EC, the Paints Directive on the limitation of volatile organic compounds: subcategory j.
Recommended use
Hempadur Avantguard 770 is recommended as a versatile primer for long-term protection of steel in severely corrosive environments. Particularly suitable for use in maintenance and offshore environments.
Service temperature
Flash point: 27°C [80°F]
VOC content mixed product
Legislation | Value |
---|---|
EU | 328 g/L [2.74 lb/US gal] |
US (coatings) | 328 g/L [2.74 lb/US gal] |
US (regulatory) | 328 g/L [2.74 lb/US gal] |
China | 328 g/L [2.74 lb/US gal] |
According to specific legislation, see Explanatory Notes on hempel.com.
Handling
Handle with care. Observe safety labels. Follow local and national safety regulations. Always consult the Safety Data Sheet along with this Product Data Sheet.
For professional use only.
Cleanliness
New build
Maintenance and Repair
Roughness
Mixing ratio
Base 17388 : Curing Agent 98384 = 4:1 by volume
Thinner
Cleaner
Pot life
Temperature | Pot life |
---|---|
20°C [68°F] | 7 hours |
40°C [104°F] | 5 hours |
Application method
Tool | Max Thinning | Parameters |
---|---|---|
Airless spray | 10% | 220 bar, 0.017–0.021″ nozzle |
Brush/Roller | 10% | Additional coats needed for film thickness |
Category | DFT (micron/mil) | WFT (micron/mil) | Spreading rate m²/L (sq ft/US gal) |
---|---|---|---|
Low | 40 / 1.6 | 61 / 2.4 | 16 / 652 |
High | 100 / 4.0 | 152 / 6.1 | 6.6 / 269 |
Recommended | 60 / 2.4 | 91 / 3.6 | 11 / 448 |
Do not exceed 200 micron [8.0 mils]. Use care on irregular surfaces.
Continuing the full content of Hempadur Avantguard 770 with drying, overcoating, storage, and the final References section — fully intact and WooCommerce/WordPress-ready:
Drying time
Surface Temperature | Touch dry | Hard dry |
---|---|---|
-10°C [14°F] | 120 min | 8.5 h |
0°C [32°F] | 60 min | 5.5 h |
20°C [68°F] | 15 min | 2.5 h |
40°C [104°F] | 5 min | 1 h |
Based on 60 µm [2.4 mils] DFT. See Hempel’s Explanatory Notes for conditions.
Quality Name and System | -10°C | 0°C | 20°C | 40°C |
---|---|---|---|---|
Atmospheric medium | ||||
Hempaprime Multi 500 Winter | 3h / Ext* | 90m / Ext* | 45m / Ext* | 25m / Ext* |
Hempathane HS 55610 | 3h / Ext* | 90m / Ext* | 45m / Ext* | 25m / Ext* |
Atmospheric severe | ||||
Hempaprime Multi 500 Winter | 3h / 90d | 90m / 90d | 45m / 30d | 25m / 7d |
Hempathane HS 55610 | 3h / 90d | 90m / 90d | 45m / 30d | 25m / 7d |
*Ext = Extended, depending on exposure. Contact Hempel for more info.
If overcoating time exceeds max, roughening is required.
Remove any zinc salts or contamination.
Temperature | Base shelf life | Curing agent shelf life |
---|---|---|
25°C [77°F] | 12 months | 36 months |
Store unopened in original containers. Do not exceed 40°C. Reinspect after expiry.
Dry Film Thickness | GWP (CO₂e) |
---|---|
1 µm | 20.5 g/m² |
1 mil | 0.107 lb/ft² |
Based on standard shade. Includes raw materials, VOCs, production, and shipping.
Product Data Sheet – Hempadur Avantguard 770
Issued by Hempel A/S – November 2024
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations