Description
Hempel’s Galvosil Fibre 15750 is a solvent-borne, self-curing, fibre reinforced, inorganic zinc silicate primer with outstanding resistance against weathering and abrasion. Provides expanded tolerance to high film thicknesses and offers excellent galvanic protection of local mechanical damage.
The product is in compliance with the compositional requirements of SSPC Paint 20 level 2 and ISO 12944 Part 5, 2018. In full compliance with ISO 3549 and ASTM D520 type II.
Recommended use
Hempel’s Galvosil Fibre 15750 is recommended as a general purpose, heavy-duty, rust-preventing primer for newbuild and maintenance. Suitable for structural steel and piping. Recommended for a wide range of atmospheric corrosivity environments up to extreme (offshore).
Can be used as a single, complete coating for long-term protection of steel exposed to moderately to severely corrosive environment and abrasion. Especially recommended for steelwork where local areas (e.g. corners) can be expected to have high film thickness (up to a dry film thickness of 200 microns).
Service temperature:
Flash point
14°C [57°F]
VOC content mixed product
Legislation | Value |
---|---|
EU | 458 g/L [3.82 lb/US gal] |
US (coatings) | 535 g/L [4.46 lb/US gal] |
US (regulatory) | 545 g/L [4.55 lb/US gal] |
China | 535 g/L [4.46 lb/US gal] |
According to specific legislation, see details in the Explanatory Notes available at Hempel website, hempel.com or at your local Hempel website.
Handling
Handle with care. Before and during use, observe safety labels on packaging and paint containers and follow all local and national safety regulations. Always consult Hempel’s Safety Data Sheet for this product along with the Product Data Sheet.
For professional use only.
Cleanliness
New build:
Maintenance and Repair
Roughness
Consult Hempel’s separate Surface Preparation Guidelines for more details.
Mixing ratio
Base 15759 : Zinc 97170 (9.2 : 15 by weight)
Products containing floating or settling particles/pigments need to be continuously stirred during application. This is especially important in case of heavy thinning.
Thinner
Hempel’s Thinner 08700
Cleaner
Hempel’s Thinner 08700
Pot life
Product temperature | Pot life |
---|---|
10°C [50°F] | 8 hours |
20°C [68°F] | 4 hours |
Application method
Tool | Thinning max vol. | Application parameters |
---|---|---|
Airless spray | 30% | Nozzle pressure: 100 bar [1500 psi], Nozzle orifice: 0.019–0.023″ |
Air spray | 35% | Not Applicable |
Brush | 10% | Not Applicable |
To minimise dry spray at high temperatures, extra thinning may be necessary.
If brush or roller application is used, more coats will be necessary to achieve the specified dry film thickness. Spray data are indicative and subject to adjustment. Pressure is for a material temperature of 20°C [68°F].
Specification range | Dry film thickness | Wet film thickness | Theoretical spreading rate |
---|---|---|---|
Low | 40 micron [1.6 mils] | 64 micron [2.6 mils] | 16 m²/L [652 sq ft/US gal] |
High | 125 micron [5.0 mils] | 201 micron [8.1 mils] | 5 m²/L [204 sq ft/US gal] |
Recommended | 75 micron [3.0 mils] | 121 micron [4.8 mils] | 8.3 m²/L [338 sq ft/US gal] |
Overthickness must be closely controlled and never locally exceed 250 micron [10 mils] DFT.
On irregular surfaces it is recommended to employ special care in avoiding over application.
Application remarks
Product compatibility
Drying time
Surface temperature | Touch dry (min) | Fully cured (hours) |
---|---|---|
0°C [32°F] | 90 | 48 |
10°C [50°F] | 40 | 23 |
20°C [68°F] | 15 | 10 |
30°C [86°F] | 6 | 5 |
Determined for dry film thickness 75 micron [3.0 mils] at standard conditions, see Hempel’s Explanatory Notes for details. The drying times of moisture curing products will depend on the relative humidity, therefore drying times in the field could vary.
Drying conditions
Overcoating details
Shelf life
Ambient temperature | Base | Zinc |
---|---|---|
25°C [77°F] | 6 months | 36 months |
Shelf life from date of production, when stored in original, unopened containers. Thereafter, the product quality must be re-inspected. Storage at elevated temperatures may reduce shelf life. For advice, please consult Hempel.
Dry film thickness | GWP (Global Warming Potential) |
---|---|
1 µm | 19.3 g CO₂e/m² |
1 mil | 0.1 lb CO₂e/ft² |
The carbon footprint is for 1 square meter / square foot of surface area with a dry film thickness of 1 micron / mil.
The scope includes raw materials, in-bound transport to the Hempel factory, Hempel manufacturing processes, and any Volatile Organic Compounds emitted during and after the application of the product.
It is calculated based on the standard shade defined in this PDS. Values may vary with shade.
Product Data Sheet –Galvosil Fibre 15750
Issued by Hempel A/S – October 2024
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations.